Material cylinder barrel |
|
Wrought aluminium alloy Smooth anodised |
|
Material cover |
|
Aluminium Anodised |
|
Pneumatic connection |
|
M5 |
|
Additional weight per 10 mm stroke |
|
21 g |
|
Additional moving mass per 10 mm stroke |
|
6 g |
|
Theoretical force at 0.6 MPa (6 bar, 87 psi), advance stroke |
|
141 N ... 188 N |
|
Ambient temperature |
|
-40 °C ... 120 °C |
|
Suitability for the production of Li-ion batteries |
|
Metals with more than 1% copper, zinc or nickel by mass are excluded from use. Exceptions are nickel in steel, chemically nickel-plated surfaces, printed circuit boards, cables, electrical plug connectors and coils |
|
Corrosion resistance class CRC |
|
0 - No corrosion stress 2 - Moderate corrosion stress 3 - high corrosion stress |
Inquiry - ADN-20-15-A-P-A-S2 (536233)